Skip to content
Home
About Us
Resources
Profiles Metrics
Authors Directory
Institutions Directory
Top Authors
Top Institutions
Top Sponsors
AI Digest
Contact Us
Menu
Home
About Us
Resources
Profiles Metrics
Authors Directory
Institutions Directory
Top Authors
Top Institutions
Top Sponsors
AI Digest
Contact Us
Home
About Us
Resources
Profiles Metrics
Authors Directory
Institutions Directory
Top Authors
Top Institutions
Top Sponsors
AI Digest
Contact Us
Menu
Home
About Us
Resources
Profiles Metrics
Authors Directory
Institutions Directory
Top Authors
Top Institutions
Top Sponsors
AI Digest
Contact Us
Publication Details
AFRICAN RESEARCH NEXUS
SHINING A SPOTLIGHT ON AFRICAN RESEARCH
engineering
Microtensile bond strength of different components of core veneered all-ceramic restorations
Dental Materials, Volume 21, No. 10, Year 2005
Notification
URL copied to clipboard!
Description
The present study aims to evaluate the core-veneer bond strength and the cohesive strength of the components of three commercial layered all-ceramic systems. Two surface treatments for the core surface finish and different veneering ceramics with different thermal expansion coefficients (TEC) were applied. The selected systems were two CAD-CAM ceramics; Cercon® and Vita Mark II and one pressable system; IPSEmpress 2 for layering technique. Standardized core specimens were fabricated according to the manufacturer's instructions, or polished with 1200 siliconcarbide polishing paper. The core specimens were veneered with either its manufacturer's veneer or an experimental veneer with higher TEC. The obtained micro-bars were subjected to the microtensile bond strength test. The obtained data were analyzed using one and two-way ANOVA. A finite element analysis (FEA) model of the test setup was analyzed. Scanning Electron Microscopy (SEM) was carried out at the fracture surface. The core materials were significantly stronger than the veneering materials and the layered core-veneer specimens of which the results were statistically comparable. Polishing the core surfaces did not have an effect on the core-veneer bond strength. Experimental veneer with higher TEC resulted in massive fractures in both the core and veneering material. SEM and FEA demonstrated fracture pattern and mechanism of failure. The core-veneer bond strength is one of the weakest links of layered all-ceramic restorations and has a significant role in their success. To exploit fully the high strength of zirconium oxide cores, further research work is needed to improve its bond with its corresponding veneering material. © 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Authors & Co-Authors
Aboushelib, Moustafa Nabil M.
Netherlands, Amsterdam
Vrije Universiteit Amsterdam
de Jager, Niek
Netherlands, Amsterdam
Vrije Universiteit Amsterdam
Kleverlaan, Cornelis J.
Netherlands, Amsterdam
Vrije Universiteit Amsterdam
Feilzer, Albert Joseph
Netherlands, Amsterdam
Vrije Universiteit Amsterdam
Statistics
Citations: 235
Authors: 4
Affiliations: 1
Identifiers
Doi:
10.1016/j.dental.2005.03.013
ISSN:
01095641
Research Areas
Health System And Policy
Violence And Injury